Easy 10-20 min PLAPETGTPU
Nozzle Oozing
Molten filament leaks from the nozzle before printing or during pauses.
Likely causes
Nozzle temperature is too high
Lower standby or print temperature. Oozing usually gets worse when the nozzle waits hot for too long.
Filament is wet
Dry the filament and store it sealed. Wet material can foam and push plastic out of the nozzle.
Retraction or wipe settings need tuning
Increase retraction slightly and use wipe or coasting features carefully if your slicer supports them.
Recommended settings by material
| Material | Nozzle | Bed | Fan |
|---|---|---|---|
| PLA | 195-210 C | 50-60 C | 80-100% |
| PETG | 230-245 C | 70-80 C | 30-60% |
| TPU | 220-235 C | 40-50 C | 30-50% |
| ABS | 240-260 C | 95-110 C | 0-30% |
| ASA | 240-260 C | 95-110 C | 0-30% |
Prevention tips
Change one setting at a time and reprint a small test piece.
Keep filament dry and store open spools in sealed bags or dry boxes.
Clean the build plate regularly and verify the correct slicer profile before long prints.
Related problems
Last reviewed Jun 15, 2026. Troubleshooting content is for reference only.